SWEDISH 5 YEARS IN-GROUND FIELD TEST, INDEX OF DECAY
Heat treatment significantly decreases the decay of wood. Results of five-year field tests for pine treated at 220 C. Source: Epmeier, Westin, Rapp and Nilsson 2003.
Heat treatment significantly decreases the decay of wood. Results of five-year field tests for pine treated at 220 C. Source: Epmeier, Westin, Rapp and Nilsson 2003.